The bonding effectiveness of five luting resin cements to the IPS empress 2 all ceramic system

Please note that UPSpace will be unavailable from Friday, 2 May at 18:00 (South African Time) until Sunday, 4 May at 20:00 due to scheduled system upgrades. We apologise for any inconvenience this may cause and appreciate your understanding.

Show simple item record

dc.contributor.author Bookhan, Vinesh
dc.contributor.author Essop, A.R.
dc.contributor.author Du Preez, I.C.
dc.date.accessioned 2019-05-09T13:28:51Z
dc.date.available 2019-05-09T13:28:51Z
dc.date.issued 2005-04
dc.description.abstract BACKGROUND : Variolink II is the only resin cement used for bonding IPS (Ivoclar Porcelain System) Empress 2 ceramic restorations. Alternative luting resin cements need to be investigated for their bonding effectiveness with the IPS Empress 2 ceramic. OBJECTIVES : To determine the shear bond strength (SBS) and the effect of thermocycling, on the bonding effectiveness, of five resin cements to IPS Empress 2 ceramic. MATERIALS AND METHODS : The projecting surfaces of one hundred ceramic discs were ground wet on silicone carbide paper. The specimens were divided into 5 groups of 20. The resin cements were bonded to the prepared ceramic surfaces, in the form of a stub. The specimens were stored under distilled water at 37°C in an oven for 24 hours. Ten specimens in each group were thermocycled for 300 cycles between 5°C and 55°C. All the specimens were stressed to failure in an Instron Materials Testing Machine. RESULTS : The results were subjected to a one-way analysis of variance (ANOVA). Statistically similar mean SBS values were grouped using the Bonferroni (Dunn) multiple comparison test. The means for the non-thermocycled group were: 26.21, 19.41, 17.69, 17.43, and 15.76. The means for the thermocycled group were: 22.90, 15.72, 14.34, 13.96 and 13.45. The differences between the means were highly significant (p< 0.0125). CONCLUSIONS : The shear bond strength of Variolink II and Rely X ARC to IPS Empress 2 ceramic was effective. Thermocycling had a significant effect on the mean SBS values of Calibra. Thermocycling had no significant effect on the mean SBS values of the other resin cements. en_ZA
dc.description.department Odontology en_ZA
dc.description.librarian am2019 en_ZA
dc.description.uri https://www.sada.co.za en_ZA
dc.identifier.citation Bookhan, V., Essop, A.R. & Du Preez, I.C. 2005, 'The bonding effectiveness of five luting resin cements to the IPS empress 2 all ceramic system', South African Dental Journal, vol. 60, no. 3, art 103, pp. 105-107. en_ZA
dc.identifier.issn 1029-4864 (print)
dc.identifier.issn 2519-0105 (online)
dc.identifier.uri http://hdl.handle.net/2263/69082
dc.language.iso en en_ZA
dc.publisher South African Dental Association en_ZA
dc.rights © 2005 E-Doc cc en_ZA
dc.subject Resin cements en_ZA
dc.subject Ivoclar porcelain system (IPS) en_ZA
dc.subject Bonding effectiveness en_ZA
dc.subject Thermocycling en_ZA
dc.subject Shear bond strength (SBS) en_ZA
dc.title The bonding effectiveness of five luting resin cements to the IPS empress 2 all ceramic system en_ZA